Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® E 2010 G6 UN - PESU-GF30 - BASF

Material Data Center offers the following functions for Ultrason® E 2010 G6 UN:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason E datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Medium viscosity injection moulding grade with high rigidity and strength, 30 % glass fiber reinforced.
Abbreviated designation according to ISO 1043: PESU-GF
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 25 / * cm³/10min ISO 1133
Temperatura 360 / * °C -
Carga 10 / * kg -
Contração após a moldagem, paralelo 0.3 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.6 / * % ISO 294-4, 2577
ASTM Dados
Contração após a moldagem, paralelo 0.004 mm/mm ASTM D 955
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração - / 9800 MPa ISO 527
Tensão na ruptura - / 150 MPa ISO 527
Deformação na ruptura - / 2.3 % ISO 527
Módulo de tensão de fluência, 1h * / 9000 MPa ISO 899-1
Resistência ao impacto Charpy , +23°C - / 55 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C - / 60 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C - / 10 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C * / 9.5 kJ/m² ISO 179/1eA
ASTM Dados
Resistência à tração na ruptura 140 / - MPa ASTM D 638
Deformação na ruptura 1.9 / - % ASTM D 638
Módulo de flexão 9722 / - MPa ASTM D 790
Impacto Izod com entalhe, 1/8 in 10 / - J/m ASTM D 256
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temp. de transição vítrea, 10°C/min 225 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 223 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 224 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 217 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 15 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 45 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-0 / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade a espessura h V-0 / * class IEC 60695-11-10
Espessuras do tubo de teste 3.0 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade conforme índice de oxigênio 47.3 / * % ISO 4589-1/-2
ASTM Dados
Coef.de expansão térmica, trans. 40 E-6/K ASTM D 696
DTUL @ 66 psi 215 °C ASTM D 648
DTUL @ 264 psi 212 °C ASTM D 648
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz * / 4.3 - IEC 62631-2-1
Constante dielétrica, 1MHz * / 4.3 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz * / 20 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz * / 100 E-4 IEC 62631-2-1
Resistividade volumétrica específica * / >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / >1E15 Ohm IEC 62631-3-2
Resistência elétrica * / 37 kV/mm IEC 60243-1
Índice comparativo de linha de fuga * / 125 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.6 / * % Sim. to ISO 62
Absorção de umidade 0.6 / * % Sim. to ISO 62
Densidade 1590 / - kg/m³ ISO 1183
Densidade 1600 kg/m³ ASTM D 792
Propriedades específicas do materialSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de viscosidade 56 / * cm³/g ISO 307, 1157, 1628
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 140 °C -
Pré-secagem - tempo 4 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 350 - 390 °C -
Temperatura do molde 150 - 190 °C -
Diagrama
Viscosidade - taxa de cisalhamento , Ultrason® E 2010 G6 UN, PESU-GF30, BASF
Tensão de cisalhamento - taxa de cisalhamento , Ultrason® E 2010 G6 UN, PESU-GF30, BASF
Módulo de cisalhamento dinâmico - temperatura , Ultrason® E 2010 G6 UN (dry), PESU-GF30, BASF
Tensão - deformação , Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Módulo secante - deformação , Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Tensão - deformação (isocrônico) 23°C, Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Módulo de fluência - tempo 23°C, Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Curva de fluencia 23°C, Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Tensão - deformação (isocrônico) 180°C, Ultrason® E 2010 G6 UN (dry), PESU-GF30, BASF
Módulo de fluência - tempo 180°C, Ultrason® E 2010 G6 UN (dry), PESU-GF30, BASF
Curva de fluencia 180°C, Ultrason® E 2010 G6 UN (dry), PESU-GF30, BASF
Volume específico - temperatura (pvT) , Ultrason® E 2010 G6 UN, PESU-GF30, BASF
Módulo de tração - temperatura , Ultrason® E 2010 G6 UN (cond.), PESU-GF30, BASF
Fatigue strength , Ultrason® E 2010 G6 UN, PESU-GF30, BASF
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão de chapas
Forma de entrega
Granulos, Cor natural
Características especiais
Galvanizável
Disponibilidade regional
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 350 - 390 °C
injection molding, Melt temperature, recommended: 370 °C
injection molding, Mold temperature, range: 150 - 190 °C
injection molding, Mold temperature, recommended: 170 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.